5.2.29 Slake Durability of Shale and Weak Rock

Laboratory testing is the scientific foundation of every geotechnical design.
Authors: Daniel P. Colwell and Mario Ruel
5.2.29 Slake Durability of Shale and Weak Rock

Shales, mudstones and claystones that look sound when cut can break down within months of exposure to wetting and drying. In railroad cuts this produces raveling, undercutting of harder beds and rockfall onto the track; as fill or riprap such rock turns to clay. The slake durability test measures that resistance by tumbling oven-dried lumps in a mesh drum half immersed in water; the second-cycle index, Id2, is the standard reporting value.

5.2.29.1 Method

Equation 5.2-14. Slake durability index

Id1 = (B − D)/(A − D) × 100;   Id2 = (C − D)/(A − D) × 100

A = drum + oven-dry sample before the test; B, C = drum + oven-dry retained material after the first and second 10-minute cycles; D = empty drum. ASTM D4644 (withdrawn 2025); ISRM suggested method.

Table 5.2-17. Slake durability classifications
First cycle Id1 (Franklin and Chandra, 1972)ClassSecond cycle Id2 (Gamble, 1971)Class
0–25%Very low0–30%Very low
25–50%Low30–60%Low
50–75%Medium60–85%Medium
75–90%High85–95%Medium high
90–95%Very high95–98%High
95–100%Extremely high98–100%Very high

Nagaraj (1993, Table 9.7) reprints the first-cycle classes with “high” and “very high” interchanged; the order above follows the original. Morgenstern and Eigenbrod (1974) also classify the amount of slaking by the liquid limit of the slaked material: very low below 20%, low 20 to 50%, medium 50 to 90%, high 90 to 140%, very high above 140%.

5.2.29.2 Worked example

Example 5.2-11: Durability of a Shale in a Rock Cut

Ten lumps of gray shale from a cut on a Class I railroad located in Pennsylvania were tested to decide whether the face needs protection. The masses are illustrative of a typical laboratory result.

Mesh drum half-immersed, 20 rpm for 10 min per cycledrum D = 1,220 gGivenDrum 1,220 g; drum + sample 1,715 gAfter cycle 1: 1,652 gAfter cycle 2: 1,571 g; LL = 38%RequiredId1, Id2Durability class
Slake durability: oven-dry lumps tumble in a mesh drum half-immersed in water; the fraction retained after two wet-dry cycles is Id2.

Given

VariableValueDescription
D1,220.0 gEmpty drum
A1,715.0 gDrum + oven-dry sample
B1,652.0 gAfter cycle 1
C1,571.0 gAfter cycle 2
LL38%Slaked fines

Required

  • Id1 and Id2
  • Durability and slaking classes

Equations

  1. Eq. 5.2-14: Id1 = (B − D)/(A − D) × 100
  2. Eq. 5.2-14: Id2 = (C − D)/(A − D) × 100
  3. Table 5.2-17: Classes

Steps

Step 1 · Sample mass
1,715.0 − 1,220.0
495.0 g
↓
Step 2 · First cycle
(1,652.0 − 1,220.0)/495.0 × 100
Id1 = 87.3%: high
↓
Step 3 · Second cycle
(1,571.0 − 1,220.0)/495.0 × 100
Id2 = 70.9%: medium
Spot check: The second cycle lost 81 g against 63 g in the first: the breakdown is accelerating, as it does in shales that soften with each wetting.
↓
Step 4 · Slaking amount
LL = 38% (20 to 50%)
Low
↓
Solution
Id2 = 70.9%: medium durability (Gamble).

Solution

The shale has medium durability (Id2 = 71%): it will weather noticeably once exposed.

In the cut, expect the shale to ravel back and undercut any harder sandstone beds above it; plan for a catchment ditch sized for that debris (rock fall hazard rating, Section 3.8.29), consider shotcrete or drapery on the shale band, and do not use the excavated shale as riprap or rockfill.

Open the slake durability calculator →
First- and second-cycle slake durability indices with the Franklin and Chandra and Gamble classes, the fragment type and the slaking class by liquid limit.

5.2.29.3 Sources

Procedures are summarized in original wording; equations and tabulated values are standard or published. Sample data are those printed in the cited laboratory manual unless stated otherwise.

  • T.S. Nagaraj, Principles of Testing Soils, Rocks and Concrete, Elsevier (1993): Section 9.5.1 and Tables 9.6 and 9.7.Find source ↗
  • J.A. Franklin and R. Chandra (1972), The slake-durability test, International Journal of Rock Mechanics and Mining Sciences, 9, 325–341.Find source ↗
  • J.C. Gamble (1971), Durability-plasticity classification of shales and other argillaceous rocks, Ph.D. thesis, University of Illinois.Find source ↗
  • N.R. Morgenstern and K.D. Eigenbrod (1974), Classification of argillaceous soils and rocks, Journal of the Geotechnical Engineering Division, ASCE, 100(GT10).Find source ↗
  • ASTM D4644 (withdrawn 2025), Slake Durability of Shales and Other Similar Weak Rocks.Official page ↗