Compaction acceptance is based on relative compaction (RC) referenced to the laboratory maximum dry density (MDD):
RC = (γ_d,field / γ_d,max) × 100%
where:
Owner railroads commonly specify Modified Proctor (ASTM D1557) as the reference for embankment, blanket layer, and subballast compaction; some specify Standard Proctor (Section 5.3.2.5). Standard Proctor is sometimes used for structure backfill behind retaining walls.
Compaction requirements:
These requirements vary by owner railroad. Confirm them against the owner railroad's current standards when the work is scoped, and record the edition used.
From the plastic limit. For red tropical (lateritic) soils, Morin and Todor (1977) related optimum moisture content to the plastic limit, and maximum dry density to optimum moisture content (standard compaction):
OMC ≈ 0.61 PL − 0.84 (South American soils; standard deviation 3.4 points)
OMC ≈ 0.58 PL − 4.54 (African soils; standard deviation 4.2 points)
MDD ≈ 163 − 2.85 OMC (pcf; African soils; standard deviation 5.5 pcf)
The density equation is converted from MDD = 25.63 − 0.448 OMC (kN/m³). The book prints it as 2563 − 4.48 OMC, but the plotted line matches the corrected form. The two OMC lines differ by about 5 points for the same plastic limit, and the scatter is large. Treat these as a first guess for borrow-source screening, not as a reference density.
The one-point method. Woods and Litehiser (1938) found that more than 10,000 compaction tests on Ohio soils fell on a family of 26 characteristic curves (Table 5.3-18). One compacted specimen, near and preferably dry of optimum, is enough to pick the curve and read the MDD and OMC. The same idea is standardized as AASHTO T 272, which uses a family of curves built from the project’s own Proctor tests. Check the family against full compaction tests before relying on it. It does not apply to uniformly graded sand, highly micaceous soils, diatomaceous earth, volcanic soils, or soils whose specific gravity is far from 2.67. Clean sands often show no clear optimum and may reach their peak density when dry.
| Curve | MDD (pcf) | OMC (%) | Wet unit weight at optimum (pcf) | Curve | MDD (pcf) | OMC (%) | Wet unit weight at optimum (pcf) |
|---|---|---|---|---|---|---|---|
| A | 141.7 | 6.6 | 151.1 | N | 109.9 | 16.9 | 128.4 |
| B | 139.2 | 7.2 | 149.2 | O | 107.4 | 18.1 | 126.8 |
| C | 136.1 | 7.9 | 146.8 | P | 104.9 | 19.2 | 125.0 |
| D | 134.2 | 8.5 | 145.6 | Q | 102.4 | 20.3 | 123.2 |
| E | 132.3 | 9.0 | 144.3 | R | 99.9 | 21.5 | 121.4 |
| F | 129.2 | 9.7 | 141.8 | S | 97.4 | 22.7 | 119.5 |
| G | 126.7 | 10.5 | 140.0 | T | 94.9 | 24.4 | 118.0 |
| H | 124.2 | 11.2 | 138.1 | U | 92.4 | 25.8 | 116.2 |
| I | 121.7 | 11.9 | 136.2 | V | 89.9 | 27.4 | 114.5 |
| J | 119.2 | 12.7 | 134.4 | W | 87.4 | 29.5 | 113.2 |
| K | 116.7 | 13.5 | 132.5 | X | 84.9 | 30.5 | 110.8 |
| L | 114.2 | 14.6 | 130.9 | Y | 83.0 | 31.5 | 109.2 |
| M | 111.7 | 15.8 | 129.4 | Z | 81.2 | 32.5 | 107.5 |
The original curves plot wet (bulk) density against moisture content. Only the peaks are tabulated here; to use the method, plot the one-point result on the original curve family or on a project family built under AASHTO T 272. Wet unit weight at optimum = MDD × (1 + OMC).
A plausibility check for any estimate. At optimum, compacted fine-grained soils are typically about 80 to 90% saturated. The Woods and Litehiser peaks sit near 84% (curve K, Gs = 2.67). An estimated MDD and OMC pair that plots on or above the zero-air-voids line, γzav = Gsγw/(1 + wGs), is impossible and should be discarded (Example 5.3-10).
For railroad work: Use the plastic-limit relations and the curve family to screen borrow sources for embankment widening and subgrade replacement, and to catch a wrong Proctor reference in the field. Where field densities run well above 100% or well below 90% of the assigned MDD, a one-point test on the material actually being placed will usually show that the soil has changed and that the reference curve must change with it. Acceptance itself must rest on a Proctor test (ASTM D698 or D1557, as the owner railroad specifies) on the material being placed.
Source: Carter, M. and Bentley, S. P. (2016). Soil Properties and their Correlations, 2nd ed., §3.2.1–3.2.2, Figs. 3.3–3.5. Summarized and paraphrased; equations and curve values converted to US units. Full reference under Supplemental References.
A Class I railroad located in Georgia is widening an embankment for a passing siding using a red, iron-rich residual clay from a nearby borrow pit. The Proctor results are a week away, but placement has started. A borrow sample has a plastic limit of 28, and a nuclear gauge test on the first lift gives a dry unit weight of 108 pcf at 17% moisture. The engineer must estimate the optimum moisture and maximum dry density from the plastic limit, check whether those estimates are possible, and decide whether the first lift can be judged against them.
| Variable | Value | Description |
|---|---|---|
| PL | 28 | Plastic limit of the borrow sample |
| γd,field | 108 pcf | Nuclear gauge dry unit weight, first lift |
| wfield | 17% | Nuclear gauge moisture, first lift |
| Gs | 2.75 | Assumed for an iron-rich residual clay |
(a) OMC ≈ 11.7 to 16.2% and MDD ≈ 117 to 130 pcf. (b) The estimates plot at about 95% and 100% saturation, which is not possible at optimum. (c) The lift would be at 83 to 92% relative compaction. (d) The lift cannot be accepted or rejected on these estimates.
Real optima lie at about 80 to 90% saturation, so both correlated points are too dense for their moisture content. The correlations were fitted to tropical soils in other countries, and with standard deviations of 4 points in OMC and 5.5 pcf in MDD they cannot decide acceptance against a 95% requirement. The field point itself, at 79% saturation and 17% moisture, looks like a reasonable compacted lean clay. The quickest way forward is a one-point compaction test on the material being placed, checked against a project family of curves (AASHTO T 272), followed by the full Proctor. Until then, keep placement to a short test section and record the gauge results, so they can be re-evaluated against the correct reference.
The nuclear gauge measures in-place density and moisture content using two radioactive sources: a cesium-137 gamma source for density (in backscatter or direct transmission) and an americium-241/beryllium neutron source for moisture. The gauge reports:
The gauge converts its count ratios to wet density (WD) and moisture using its calibration.
In practice, results are read directly from the calibrated gauge display. Field procedure:

Gauge standardization and calibration: ASTM D6938 requires a standard count on the reference block each day of use and gauge calibration at least every 12 months. Nuclear gauges are licensed NRC devices; technician must hold current radiation safety training certification. Carry the license documents and the operator's training card in the field as the license conditions require.
Correction for materials containing significant gravel or rock: use ASTM D4718, which corrects the laboratory maximum dry density for the oversize fraction retained on the ¾-in. sieve (generally applicable up to about 30% oversize):
γ_d,max,corrected = 100 γ_d,f (G_m γ_w) / (γ_d,f P_c + G_m γ_w P_f) (pcf)
where γ_d,f = maximum dry unit weight of the finer fraction; G_m = bulk specific gravity of the oversize; P_c, P_f = percent oversize and finer fraction (by dry mass).
The sand cone method is commonly required for acceptance testing in compacted structural fill adjacent to structures and retaining walls, and as the verification method when nuclear gauge results are disputed.
Field bulk density:
ρ_bulk = (M_soil) / V_hole (pcf)
Volume of hole:
V_hole = (M_cone−sand,initial − M_cone−sand,final − M_sand,funnel) / ρ_sand,calibrated (ft³)
Dry density:
γ_d = ρ_bulk / (1 + w/100) (pcf)
where w = gravimetric water content (%) from oven-dried sample (ASTM D2216).
Sand cone testing is slower than nuclear gauge but is considered the more accurate reference method. Minimum test frequency varies by owner (1 test per 500 to 1,000 cy of compacted fill is common); confirm with the project specification.
| Symbol | What it is | Comes from | How to get it | Typical range |
|---|---|---|---|---|
| ρbulk | intermediate value computed on this page | Another equation | Computed: ρ_bulk = ( M_soil ) / V_hole (pcf) | project-specific |
| Vhole | intermediate value computed on this page | Another equation | Computed: V_hole = ( M_cone−sand,initial − M_cone−sand,final − M_sand,funnel ) / ρ_sand,calibrated (ft³) | project-specific |
| γd | dry unit weight = ρ_bulk / (1 + w/100) (pcf) | Lab or field test | Lab: ASTM D7263 on tube samples. Field: nuclear gauge (ASTM D6938), sand cone (D1556) or drive cylinder (D2937). Or γd = γ/(1 + w). | sands 90–125, clays 80–115 pcf · by USCS group |
| w | water content | Lab test | Oven-dry water content of samples (ASTM D2216); field check by microwave (D4643) or nuclear gauge (D6938). | gravels/sands 3–25%, clays 15–70% · by USCS group |
| Application | Frequency | Trigger for Retest |
|---|---|---|
| Embankment lift (main body) | 1 test per 500 ft of track per lift | RC < minimum |
| Blanket layer / subgrade prep | 1 test per 250 ft of track per lift | RC < minimum |
| Structural fill (bridge abutment) | 1 test per 2 ft lift per 50 ft length | RC < minimum |
| MSE wall reinforced fill | 1 test per 2 ft lift per 100 ft | RC < minimum |
| Retaining wall backfill | 1 test per 2 ft lift per 50 ft | RC < minimum |
| Trench backfill (pipe, drain) | 1 test per 50 linear ft per lift | RC < minimum |

Source: typical practice. Confirm testing frequencies against the owner railroad's standards and the project specification.
The purpose of compaction is to gain strength and stiffness, reduce compressibility, plastic strain under repeated load, permeability and swell. Density is just the convenient thing to specify. Keep these points in mind when setting and checking specifications:
After Selig & Waters (1994), chs. 9 and 11. Full reference under Supplemental References.
Spot tests sample a tiny fraction of a lift. Roller-integrated measurement covers 100% of the area and can find soft zones deeper than a nuclear gauge. SHRP2 distinguishes CCC (the roller records a drum-response stiffness value with GPS position) from intelligent compaction (the roller also adjusts amplitude, frequency or speed automatically). It is best suited to granular fills, sand, crushed gravel and rock fill — i.e., subballast and embankment granular layers. The Austrian contractual provisions summarized by Adam (2007) show how to make it an acceptance test:
A falling roller value on repeated passes indicates loosening, particle crushing or pore pressure build-up — a reason to stop rolling, not to add passes.
Source: Adam, D. (2007). “Roller-integrated Continuous Compaction Control (CCC): Technical Contractual Provisions & Recommendations.” In Gomes Correia, A., Momoya, Y. and Tatsuoka, F. (eds.), Design and Construction of Pavements and Rail Tracks. Taylor & Francis/Balkema · SHRP2 R02 / GeoTechTools (2012). Intelligent Compaction — technology fact sheet
UIC practice compacts the formation layer (the improved top-of-subgrade layer over S1 or S2 subsoil) to 100% of Standard Proctor, compared with 95% routinely specified for embankment subsoil. The formation layer also has to be homogeneous, without local concentrations of fine material, and placed on subsoil with a low water content. Otherwise subsoil fines migrate into it and the 3–5% crossfall is lost. Field QA should therefore watch uniformity and subsoil moisture as well as density.







After Profillidis (2014), §9.7.1. Full reference under Supplemental References.
Profillidis sets two checks before track laying begins: the subgrade has been properly compacted, and the 3–5% crossfall is correctly formed. Ballast is then delivered by special wagons, placed, levelled, graded and consolidated with a vibrating plate or roller. Uniform tie spacing matters as much as the nominal spacing. A high-speed laying machine averages about 0.81 mi per 6-hour shift, with peaks of 1,640 ft/h and 0.93–1.2 mi per shift. Once laid, the rails are set with a rail-positioning machine (Figure 5.3-11).

For the geotechnical inspector, those two checks are natural hold points. Document the subgrade density results and a crossfall survey before the contractor places ballast, because neither can be corrected afterward without removing the track.
After Profillidis (2014), §16.1.1, Fig. 16.1. Full reference under Supplemental References.
Backfill and compact every 2-ft lift; skipped lifts leave voids that resettle under traffic. Match the compactor to the soil: a smooth-drum vibratory roller for granular fill, and never a sheepsfoot on saturated silt or clay, which can liquefy. Excavate in lifts and shore or slope trenches; trench collapses kill workers every year. Wear rain gear and keep clear of live track when digging beside the rail.


After Geotechnology for Railroaders Program, Module 6.2, Module 6.1; Module 6.2 §02, §05; Module 6.1 §02. Full reference under Supplemental References.
Case study: 5.3.18.1 Field moisture ratios behind 5,649 passing density tests (Look 2023), in Section 5.3.18 Case Studies.
The library's notes on mass-volume relationships and compaction give the phase relations behind every field density test. On railroad embankments and subgrade the acceptance test is relative compaction against the Proctor maximum, usually with a moisture window around optimum; the zero-air-voids line is the check that catches a wrong Proctor curve or a misread water content, because no real test can plot above it.
Equation 5.3-1. Phase relations
Equation 5.3-2. Acceptance
| Layer | Typical requirement | Note |
|---|---|---|
| Embankment fill | 95% of standard Proctor (ASTM D698), ±2% of optimum | Lifts 8 to 12 in. loose |
| Top 2 ft of subgrade | 95 to 100% of standard Proctor | Most heavily stressed soil |
| Subballast | 95 to 100%, or a method specification | Well-graded, low fines |
| Trench and culvert backfill | 95%, hand-operated equipment near the pipe | Avoid deflecting flexible pipe |
Project specifications govern; the values above are common ranges for railroad work.
| Result | Value |
|---|---|
| Proctor maximum dry unit weight | 119.2 pcf |
| Optimum water content | 12.3 % |
| Field dry unit weight | 113.6 pcf |
| Relative compaction | 95.3 % (passes 95%) |
| Moisture relative to optimum | +0.8 % (within window) |
| Result | ACCEPT |
Open the compaction calculator →
Proctor curve fit, maximum dry unit weight and optimum water content, zero-air-voids line, field relative compaction, saturation and accept or reject against the specification.
These documents are in the reference library. The method summaries above are paraphrased; equations are standard forms.