The relationship between dry unit weight and moisture content is defined by the Proctor test. The maximum dry unit weight γ_d,max and optimum moisture content w_opt are the design targets for compaction control (Chapter 5.3).




Zero Air Voids (ZAV) line:
Where G_s = specific gravity (≈ 2.70 for most soils); γ_w = 62.4 pcf; w = water content (decimal).
Relative compaction (RC):
Standard Proctor (ASTM D698): 12,400 ft·lb/ft³ compactive effort; appropriate for light to moderate railroad facility construction. Modified Proctor (ASTM D1557): 56,000 ft·lb/ft³ compactive effort; commonly specified for intermodal yards, bridge approach fills and railroad embankments.

| Symbol | What it is | Comes from | How to get it | Typical range |
|---|---|---|---|---|
| Gs | specific gravity (≈ 2.70 for most soils) | Lab test | Specific gravity of solids (ASTM D854). 2.65–2.70 is usually adequate for mineral soils when untested. | 2.64–2.80 mineral; lower if organic · by USCS group |
| w | water content (decimal). | Lab test | Oven-dry water content of samples (ASTM D2216); field check by microwave (D4643) or nuclear gauge (D6938). | gravels/sands 3–25%, clays 15–70% · by USCS group |
Vibratory compaction (smooth drum, padfoot) densifies granular fills and coarse-grained subgrades. Compaction effectiveness is described by the influence depth Z_eff:

Where W = drum weight (lb); A_f = drum contact area (ft²); k = empirical constant (0.08–0.12 for granular materials).
Lift thickness limits by soil type:
| Symbol | What it is | Comes from | How to get it | Typical range |
|---|---|---|---|---|
| W | drum weight (lb) | Loading criteria | From the loading criteria: AREMA MRE (Cooper E-80, impact), structural loads from the designer, or equipment specifications. | project-specific |
| Af | drum contact area (ft²) | Project geometry | From project plans, survey and the design layout; layer depths and thicknesses from the boring logs. | project-specific |
| k | empirical constant (0.08–0.12 for granular materials). | Chart, table or correction factor | Read from the cited chart or table for the site conditions; values listed in the definition. | project-specific |
Dynamic compaction densifies loose fills and granular soils by repeated high-energy drops of a heavy pounder (10,000–30,000 lb) from heights of 30–90 ft.


Influence depth (Menard & Broise 1975):
Where (metric, as published; multiply D by 3.28 for feet):
Energy per unit area:
For railroad applications, dynamic compaction is restricted to areas beyond client setback from active track (Table 7.2-1). Vibration monitoring (Chapter 5.3) with a peak particle velocity (PPV) threshold of 0.5 in./s at the nearest track is commonly required.
| Symbol | What it is | Comes from | How to get it | Typical range |
|---|---|---|---|---|
| Wh | weight of pounder (tons) | Loading criteria | From the loading criteria: AREMA MRE (Cooper E-80, impact), structural loads from the designer, or equipment specifications. | project-specific |
| H | drop height (ft) | Project geometry | From project plans, survey and the design layout; layer depths and thicknesses from the boring logs. | project-specific |
| n | empirical efficiency factor (0.35–0.65 | Chart, table or correction factor | Read from the cited chart or table for the site conditions; values listed in the definition. | project-specific |
Table 17-S2. Upper-bound test values after deep dynamic compaction (GEC 13, Table 4-2, from FHWA 1986)
| Soil type | SPT N (blows/ft) | CPT qc (tsf) | PMT limit pressure (tsf) |
|---|---|---|---|
| Pervious coarse-grained: sands and gravel | 30–50 | 200–300 | 20–25 |
| Semipervious: sandy silts | 25–35 | 135–177 | 14.6–20 |
| Semipervious: silts and clayey silts | 20–35 | 104–135 | 10.4–14.6 |
| Partially saturated impervious: clay fill, mine spoil | 20–40* | N/A | 14.6–20 |
| Landfills | 15–40* | N/A | 5.2–10.4 |
* Higher values may reflect large particles. These are maxima for estimating what is possible; verify actual improvement by testing while the equipment is still on site, and allow for delayed improvement as pore pressures dissipate.
Rapid impact compaction (RIC) is a smaller-footprint alternative where the setbacks in Table 7.2-1 rule out a crane and pounder. A 5–9 ton weight on an excavator drops about 4 ft onto a 5-ft-diameter tamper at 40–60 blows/min. It densifies granular fills, ash and building waste to about 10–20+ ft and covers about 9,000–30,000 ft2 per shift. Groundwater should be at least 3 ft below the surface. It is not recommended for weak, low-permeability, clayey or high-fines soils. Energy and set per blow are recorded for QC, with SPT or CPT before and after for QA. Recorded peak noise was about 88 dBA. The depth of compaction cannot be controlled precisely.





Jet grouting diameters reported by SHRP2 range from about 3 to 15 ft (larger than the 1.5–5 ft in Section 7.2.6.3, which reflects smaller systems). Depths are generally under 100 ft but exceed 160 ft in some cases. Soilcrete strength reflects the soil (higher in sands and gravels). Highly plastic clays and fibrous peat erode poorly and are not recommended. Spoil must be removed continuously, and surface or lateral movement must be watched — an important check beneath or next to track.
Source: Schaefer, V. R. et al. (2017). Ground Modification Methods Reference Manual, Vol. I. Geotechnical Engineering Circular No. 13, FHWA-NHI-16-027 · SHRP2 R02 / GeoTechTools (2012). Rapid Impact Compaction and Jet Grouting fact sheets
Technology sheets for this method · see 7.2.16 Technology Library





Case study: 7.2.17.1 Measuring roller force with pile-driving monitors (Look 2023), in §17.17 Case Studies.










UK earthworks specifications control compaction in two ways. A method specification fixes the plant, layer thickness and number of passes for each material class, with daily records of what was done. An end-product specification sets a minimum compacted state that is tested in place; a layer should not be covered until it has been shown to comply (Dumelow, 2012, Section 75.5, pp. 1119–1133). AREMA and most railroad specifications are end-product (percent of maximum dry density at a moisture range), so the testing frequency and the hold on covering a layer are what make them work.
| Test | Time | Typical acceptable limit | Constraint |
|---|---|---|---|
| Moisture Condition Value (MCV) | About 15 min | 8 to 16 | Must be correlated with fundamental tests for each material; weak for granular or very silty or sandy soils |
| Hand shear vane | About 1 min | Over about 1,460 psf (70 kPa) | Not suitable for clay with much sand or gravel |
Dumelow (2012), p. 1133. Shear strength converted from kPa.
Bender-element tests on a clayey soil treated with 3% lime and compacted to a dry density of about 100 pcf (1.60 Mg/m³) found (Tang, Vu and Cui, 2011, pp. 35–44):
For lime-treated subgrade and fill, specify pulverisation (Section 7.2.7), prepare laboratory mixes at the field clod size, and protect the treated layer from drying out before it is covered.
Paraphrased from the published sources below; values are converted to English units. Individual railroads, clients and projects are not named.
A building pad in mountainous terrain sat on 6.5 to 26 ft of weathered rock and soil that had been end-dumped without compaction two years earlier. Most particles were 0.2 to 8 in., with some over 20 in., and the fill carried only about 1,500 to 2,100 psf. Treatment used two high-energy passes of about 2,200 kip-ft per drop, followed by two lighter ironing passes of about 1,100 and 740 kip-ft.
For railroad work: Old side-cast and end-dumped fills of rock and soil are common along mountain grades and at abandoned yards. The case shows that coarse, boulder-bearing fill can be brought to a reliable bearing surface by dynamic compaction where vibration limits allow it, and that GPR is a practical way to confirm the depth of improvement. Keep the vibration limits of Section 7.2.2.3 for any work near live track, signals and structures.
Source: Lu, Filz and Han (2009), in Han, J. et al. (eds.) (2009), Advances in Ground Improvement, ASCE GSP 188. Full reference under Supplemental References.
Explosives are best known in ground improvement for densifying loose saturated sand (see the blasting densification sheet in Section 7.2.16). This paper describes a different use: explosive replacement. Crushed stone is stockpiled beside the area to be treated, charges are set in the soft clay in a planned pattern, and the blast opens cavities into which the stockpile slides. Charge weight and spacing were set from blast-cavity equations.
For railroad work: Explosive replacement is a remote-site option for building a new alignment across a shallow soft clay or organic deposit where excavation and replacement would be slow. It is not suited near operating track or structures. Expect incomplete replacement at the base of the deposit and verify with borings and GPR.
Source: Yan, Dong and Chu (2009), in Han, J. et al. (eds.) (2009), Advances in Ground Improvement, ASCE GSP 188. Full reference under Supplemental References.
Dynamic replacement uses heavy tamping to drive large pillars of imported granular material into soft saturated soil. The craters are filled with stone or sand and pounded again, forming columns that both reinforce the soil and drain it. The soil between the pillars is compressed, and the excess pore pressure this creates takes hours to dissipate, so passes are spaced in time. Rotational dynamic compaction drops a tamper that also rotates as it falls; in comparative trials it penetrated about twice as far as a conventional tamper and gave higher cone resistance, increasing the depth of improvement in granular soils.
For railroad work: Both methods produce strong ground vibration and crater heave, so the setback from active track (Table 7.2-1) and the vibration limits for dynamic compaction in Section 7.2.2 apply. Dynamic replacement suits yard and access road areas on soft ground away from operating track, where its columns also speed consolidation.
Source: Singh and Hymavathi (n.d.). Full reference under Supplemental References.
Two explosive ground improvement methods appear in this chapter. Blast densification of loose saturated sand is described in the technology sheet in Section 7.2.16. Explosive replacement of soft clay is described in the box above. Both deliberately cause strong vibration and, for blast densification, temporary liquefaction of the treated layer.
For railroad work: Treat either method as blasting, not as ground improvement vibration. The same controls apply as for rock excavation blasting:
(1) the scaled-distance or monitored-PPV limits of Section 5.3.27;
(2) a seismograph at the nearest track, structure and signal equipment;
(3) the 0.5 in./s at-rail threshold in this section.
Liquefaction of the treated layer can spread to untreated loose ground beyond the treatment area, so keep these methods well clear of operating track. Use them for new alignments and yards on greenfield ground, and confirm the result by CPT several weeks after treatment, when strength gain has occurred.
Source: 30 CFR 816.61–816.68. Full reference under S23.