| Rock | Problem | Tests | Engineering response |
|---|---|---|---|
| Shale, mudstone, claystone | Slaking and softening on wetting and drying; swelling; low residual strength on bedding | Slake durability (ASTM D4644, withdrawn 2025): Id2 < 60% low durability; jar slake test; Atterberg limits of slaked material | Treat as soil in fills (compact in thin lifts, break down); protect cut faces; use fully softened or residual strength |
| Pyritic shale and slate | Oxidation of pyrite causes heave, acid drainage and sulfate attack | Sulfur and sulfate content; pH | Avoid in fill near structures; sulfate-resistant concrete; acid drainage control |
| Limestone, dolomite, gypsum (karst) | Solution cavities, sinkholes, pinnacled rock surface, collapse of soil cover | Geophysics (ERT, MASW, GPR), closely spaced probes, coring | Grouting, bridging slabs or geogrid, drainage control (do not concentrate water), avoid ponding in ditches |
| Weathered granite and gneiss (saprolite) | Corestones and boulders in soil matrix; variable depth to rock | Seismic refraction; borings with coring | Plan excavation for boulders; bearing on variable surface |
| Volcanic tuff and ash | Low density; may slake or collapse | Unit weight, slake durability | As for weak rock |
See Chapter 3.8, Section 3.8.5 for subsidence and karst collapse mechanisms.
Seismic P-wave velocity from refraction surveys (Chapter 5.1, Section 5.1.7) is the usual first indication of how rock can be excavated: velocities below about 4,000 to 5,000 ft/s are generally rippable with large dozers, about 5,000 to 8,000 ft/s may be marginal, and higher velocities usually need blasting. The limits depend on the equipment and on joint spacing; check against manufacturer rippability charts and test excavations.