| Material | γ (pcf) | Strength | Modulus | k (ft/day) | Notes |
|---|---|---|---|---|---|
| Loose SP sand | 95–110 | φ′ 29–31° | Es 200–500 ksf | 3–300 | Settles under vibration; liquefiable when saturated |
| Medium dense SP/SW sand | 105–120 | φ′ 31–36° | Es 500–1,000 ksf | 3–300 | Good fill and subballast source |
| Dense SW sand | 115–130 | φ′ 36–41° | Es 1,000–1,700 ksf | 3–300 | — |
| Silty sand SM | 110–125 | φ′ 29–34° | Es 300–800 ksf | 0.03–3 | Frost susceptible; see Chapter 2.4 |
| Shale (weak rock) | 135–155 | qu 500–5,000 psi; joints 20–30° | 0.2–1×106 psi | — | Slakes; treat as soil when weathered |
| Sandstone (medium strong) | 140–160 | qu 5,000–15,000 psi | 1–4×106 psi | — | Bedding-controlled sliding |
| Limestone (strong) | 155–170 | qu 8,000–25,000 psi | 3–8×106 psi | — | Karst |
| Granite (very strong) | 160–170 | qu 15,000–35,000 psi | 4–10×106 psi | — | Joint-controlled wedges; rockfall |
Starting values only; replace with test data and mapping.