2.4.10 Loess and Collapsible Silts

Silt sits between sand and clay: too fine to drain freely, too coarse and too weakly plastic to hold together when wet. That combination makes it the soil most often behind track pumping, frost heave, piping, sloughing cut slopes, collapsing loess and liquefaction of fine-grained ground.
Author: Daniel P. Colwell
2.4.10 Loess and Collapsible Silts

Loess is wind-deposited silt with an open structure held together by clay bridges and carbonate cement. While dry it stands in near-vertical cuts tens of feet high. When wetted under load, the bonds soften and the structure collapses, often by several percent of the layer thickness, with no added load.

Screening for collapse

Gibbs and Bara (1962): a loose silt is likely to collapse if its water content at saturation is greater than its liquid limit, because on wetting it would be weaker than a soil at the liquid limit:

wsat = γwγd − 1Gs > LL    ⇒   collapse likely

Eq. 2.4-24

Typical loess with γd below about 85 pcf and LL near 30 fails this check. Natural dry unit weights above about 100 pcf rarely collapse significantly.

Measuring collapse

ASTM D4546 (which replaced D5333, withdrawn in 2012) loads an undisturbed specimen in a consolidometer to a chosen stress, then floods it. The collapse at a stress of 4.2 ksf (the standard index stress) is the collapse index Ie; the collapse at the actual design stress is the collapse potential used to estimate settlement:

CP (%) = Δe1 + e0 × 100      Scollapse ≈ Σ CPi · Hi

Eq. 2.4-25 and Eq. 2.4-26 (sum over layers expected to wet)

Table 2.4-14: Degree of Collapse
Collapse index Ie (%) at 4.2 ksf (ASTM D4546)Degree of specimen collapseCollapse potential CP (%) (Jennings and Knight 1975)Severity of problem
0None0–1No problem
0.1–2.0Slight1–5Moderate trouble
2.1–6.0Moderate5–10Trouble
6.1–10.0Moderately severe10–20Severe trouble
> 10Severe> 20Very severe trouble

Jennings and Knight CP is measured at 4.2 ksf in the double-oedometer or single-oedometer test; the two scales are listed side by side for comparison and are not exact equivalents.

Railroad hazards in loess

  • Cut slopes. Loess cuts are stable near vertical (or in benched vertical faces) when kept dry, and fail when flattened to slopes that let rain soak in. Conventional practice is near-vertical faces with benches and crest drainage, rather than flattened slopes. Never let ditch water pond at the toe.
  • Embankments on loess. Wetting from ponded ditches, broken drain pipes or culvert leaks causes collapse settlement under the embankment. Control water first; pre-wetting or removal and recompaction are used for new fills.
  • Loess pipes and sinkholes. Water concentrated along roots, cracks or culvert bedding erodes vertical pipes and tunnels in loess; the surface expression is a sinkhole, sometimes under the track. Treat them with the piping remedies of Section 2.4.7.
  • Retaining structures. Use driven soldier piles with lagging for stabilization walls in loess cuts; keep surface water away from the lagging and provide weep drainage behind it.

Other special silts

Table 2.4-15: Special Silts and Their Problems
SiltRecognitionEngineering concern
Micaceous saprolite (Piedmont)Shiny flakes; slick feel; low unit weight for its density; ML or MHSpringy, hard to compact; high Cc and rebound; low φ′; erodible; Proctor density not achievable in the field
Diatomaceous siltVery low Gs (2.0–2.5); very high w and LL; light when dryHigh compressibility despite high φ′; misleading index tests
Varved glacial lake depositsAlternating silt and clay layers, typically less than 1 in. thickHorizontal permeability many times vertical; frost group F4; slope failures along silt partings
Sensitive (quick) silty clayLarge strength loss on remolding; St > 8; eastern Canada glacial marine depositsRetrogressive flow slides along river valleys; avoid disturbing the toe; vibration-sensitive
Organic silt (OL/OH)Dark color, odor; LL drops on oven dryingHigh compressibility and secondary compression; low strength