2.12.3 Pyrite and Sulfide Oxidation

Ground chemistry that attacks concrete, heaves stabilized subgrades and turns fresh shale into soil within a few seasons of exposure.
Author: Daniel P. Colwell
2.12.3 Pyrite and Sulfide Oxidation

Pyrite (FeS2) is common in dark shales, coal measures and some slates and organic clays. While it stays buried below the water table it is stable. When a cut or excavation exposes it to air and water it oxidizes, producing sulfuric acid, iron hydroxide staining and sulfate. The consequences are:

  • Heave: sulfate reacts with calcite in the rock to form gypsum, which occupies about twice the volume. Floor slabs, footings and backfill on pyritic shale or pyritic shale fill have heaved several inches over a few years.
  • Acid drainage: low-pH water with dissolved iron and metals from cut slopes and spoil, staining ditches orange and attacking concrete and steel.
  • Secondary sulfate attack on concrete from the sulfate produced.
  • Faster degradation of the rock itself as acid and crystal growth open fractures.

Screening tests include total sulfur, pyritic sulfur, acid-base accounting (acid-producing potential vs. neutralizing potential) and paste pH. Do not use pyritic shale as structural fill under slabs or behind walls, and do not let pyritic spoil drain to streams without treatment.